Exposed Aggregate

HOW TO ACCOMPLISH AN EXPOSED AGGREGATE FINISH STEP BY STEP USING ECOGUARD TOOLING

BOOMER MB #50/60
Soft Or Hard Concrete

TURBO MB #50/60 Medium to Medium Hard

HYPER GRIND #50/60
VERY HARD CONCRETE

STEP

1

 HG LITHIUM DENSIFIER

STEP

2

TITANIUM BM #100

STEP

3

Spray properly diluted Pore Filler on the concrete floor and grind it to a slurry using the PORE FILLER PAD #1. Grind to achieve a thin pudding-like mud consistency, and continue to grind dry until all surface residual has been ground off. .Refer to tech data for complete details. ​​

 

ECOGUARD Pore Filler

 

 

PORE FILLER PAD #1

 

STEP

4

 

WATERGLOSS #2

 

 

WATERGLOSS #3

 

STEP

5

STEP

6

 

WATERGLOSS #4 Higher Gloss and DOI

 

STEP

7

 

Use a MED. HOGS HAIR PAD to burnish

 

 

Apply POLISHIELD with microfiber applicator

 

STEP

8

Questions?