Cream Texture Finish

HOW TO ACCOMPLISH A Cream Texture Finish STEP BY STEP USING ECOGUARD TOOLING

BOOMER MB #50/60
Soft Or Hard Concrete

TURBO MB #50/60
Medium to Medium Hard

STINGRAY PUCK
#30

STEP

1

STINGRAY PUCK
#50

STEP

2

Spray properly diluted Pore Filler on the ccncrete floor and grind it to a slurry using the WATERGLOSS 100 grit. Grind to achieve a thin pudding-like mud consistency, and continue to grind dry until all surface residual has been ground off. .Refer to tech data for complete detials. ​

ECOGUARD Pore Filler

 

WATER GLOSS #100

STEP

3

WATER GLOSS #200

STEP

4

WATERGLOSS
#400

STEP

5

MAMBA #800

STEP

6

ECOGUARD POLISHIELD

STEP

7