Exposed Aggregate

HOW TO ACCOMPLISH AN EXPOSED AGGREGATE FINISH STEP BY STEP USING ECOGUARD TOOLING
BOOMER MB #50/60
Soft Or Hard Concrete
TURBO MB #50/60 Medium to Medium Hard
HYPER GRIND #50/60
VERY HARD CONCRETE
Step


1
HP COLLOIDAL or HG LITHIUM DENSIFIER
Step

2
TITANIUM BM #100
Step

3

Spray properly diluted Pore Filler on the ccncrete floor and grind it to a slurry using the PORE FILLER PAD #1. Grind to achieve a thin pudding-like mud consistency, and continue to grind dry until all surface residual has been ground off. .Refer to tech data for complete detials. ​

ECOGUARD Pore Filler
PORE FILLER PAD #1
Step

4
WATERGLOSS #2
Step

5
WATERGLOSS #3
Step

6
WATERGLOSS #4 Higher Gloss and DOI
Step

7
Use a MED. HOGS HAIR PAD to burnish
Apply POLISHIELD with microfiber applicator
Step

8